Ink

HY Series Organic Bentonite Use Method

HY series organic bentonite is made by excellent bentonite with the processing of highly purified, modified and ion exchange into organic covering agent, it is a sheet structure product, if you want the organic bentonite to play a better performance, you need to separate its sheet-structure as much as possible. This process usually needs to be provided with mechanical energy, chemical energy and heat energy.

Use Method:

Dry powder method:

Dry powder method is that add the dry powder directly into the system during the production process, it doesn't need the polar activator, such as HY-2, HY-S2, HY-S3, HY-S34.

Pre gel method:

For poor wettability resin systems (such as epoxy, polyester, short oil alkyd resin etc. )it is better to use HY series organic bentonite by pre gel. 

(1) composed of pre gel: solvent 87%, organic bentonite 8-10%, polar activator 3-4%.

(2) preparation of pre gel: solvent and organic bentonite (mixed 10min, fully wettability), then add the polar activator (stirring for 5min, full expansion). 

Other information:

The dispersion speed

No matter you use any one method, bentonite products must be thoroughly dispersed to be a gel, so it can show its properties as thixotropy, anti settling and thickening effect, this kind of dispersion need extra high shear force, for example, to use high speed dispersion machine, three roller mill, colloid mill, sand grinding or milling. If the shear force and activation energy is enough, it is easy to obtain gel. The organic bentonite efficiency increased with the increase of dispersion speed.

Dispersion temperature

Increasing the temperature can also improve the gel property. The gel property with high temperature solvent is better than the low temperature (0 °C -5 °C ) solvent when the other conditions keep the same. But the dispersion temperature can not exceed the boiling point of activation solvent.

Activating agent

The polar additive can help the sheet-layer structure bentonite easily form a layer-sheet structure, thus formed a thixotropic gel, polar additives such as ethanol, methanol, acetone, propylene carbonate, the add amount of polar additives is generally 30%-50% of the organic bentonite.

Moisture

Organic bentonite must have enough moisture to develop into a network structure pre gel, the water molecules forming a bridge for the network structure, so the organic bentonite should not be too dry, the general moisture content should be around 3.5%, polar additives should not use anhydrous, the suitable content of the polar additives is appropriate 95% (the moisture is 5%).


主站蜘蛛池模板: 精品无码午夜福利理论片| 成人亚洲精品久久久久软件| 久久日韩乱码一二三四区别| 日日碰狠狠躁久久躁蜜桃| 亚洲日韩一区二区一无码| 亚洲а∨天堂2014在线无码 | 激情偷乱人伦小说视频| 成 人 免 费 黄 色| 久久国产精久久精产国| 亚洲成在人线在线播放无码| 亚洲毛片多多影院| 国产成人精品手机在线观看| 97超碰中文字幕久久精品| 72种姿势欧美久久久久大黄蕉| av免费网址在线观看| 天天躁日日躁狠狠久久| 亚洲狠狠婷婷综合久久久久图片| 久久综合99re88久久爱| 在线视频 亚太 国产 欧美 一区二区| 40岁成熟女人牲交片| 久热在线播放中文字幕| 亚洲精品午夜一区二区电影院| 高清偷自拍第1页| 亚洲午夜无码久久久久软件| 精品综合久久久久久98| 国产精品麻豆成人av电影| 99精品国产高清一区二区麻豆 | 中文无码不卡人妻在线看| 99re6这里有精品热视频| 无码人妻一区二区三区精品视频 | 久久欧美国产伦子伦精品| 国产精品高潮呻吟av久久黄 | 97国产露脸精品国产麻豆| 无码中文字幕| 无码天堂亚洲国产av麻豆| 尹人香蕉久久99天天拍欧美p7| 久热爱精品视频线路一| 国产精品嫩草影院av | 精品av一区二区久久久| 青草青草久热精品视频观看| 亚洲中文字幕无码卡通动漫野外|